Cu-Pb-Zn Dressing Process

Process Advantages


Adopting mixed flotation-concentrate regrinding process can reduce the grinding cost, and be easy to manage. Application of new non-toxic flotation reagents is efficient and environmental protection.

Application

Mixed flotation-concentrate regrinding process is applied for Cu-Pb-Zn sulfide ore

[ Process Advantages ]

Creative process, low operation cost

Cu-Pb mixed concentrate regrinding process saves the grinding cost without fine grinding all the ores are, and it makes further monomer dissociation to create favorable conditions for the separation of copper and lead.

[Cases]

Case 1

Tibet Lead zinc Beatification Plant is one of our successful cases. This is 3D demo Video of the dressing plant created by our company.

Case 2

A lead-zinc dressing plant in Yunnan, , due to the mining depth increasing, ore properties had changed and the grade of lead and zinc concentrate decreased, so the original flotation is not suitable. After field investigation and analysis, BaoShan determined the process according to multi tests:  mixed flotation, preferential flotation of copper lead concentrate, regrinding and re-floating of copper lead concentrate, and equipped with the BaoShan equipment. Indexes comparison as follow:

Comparison of Reformation

Process

Capacity
t/d

Copper Recovery Rate 
/%

Pb Concentrate Grade/%

Zinc Concentrate Grade/%

Service Life of Equipment Liners/Day

Before Reformation

Preferential Flotation

500

78.53

35.68

83.49

50

After Reformation

Mixed Flotation

680

83.45

50.13

84.68

90

After the technical reformation, this plant increased the output value of nearly 30000 yuan/day, and the profit increasing of 26000 yuan/day. The economic benefit is remarkable.

Case 3

A copper-lead dressing plant in Xinjiang: the ore with the close symbiosis and fine particle distribution, the process the plant adopted leaded to the poor concentrate grade. So BaoShan was authorized to reform the technology.

After analysis of crude properties, BaoShan decided to adopt parts of the preferential flotation process. Firstly, selective collectors floated copper based on the original preferential flotation process; then mixed flotation and regrinding the mixed concentrate, grinding fineness can reach -38 u m78%.

BaoShan technical reformation had the advantages of simple process and low production cost; the recovery of copper concentrate was 90.21%; lead and zinc are qualified; lead concentrate had recovery rate of 88.3%. BaoShan obtained highly praise from clients.

By this cooperation, clients witnessed the good device performance and good after sale service from BaoShan. In recent years, BaoShan has more and more cooperation with large domestic enterprises, which enhances the BaoShan service level and exercise installation team. BaoShan also has finished more foreign EPC projects.

Other cases:

There are many cases of BaoShan Cu-Pb-Zn Dressing Process. Welcome to visit our company!

A copper-lead-zinc dressing plant in northwest of China, BaoShan adopted parts preferential flotation based on technology advantages of preferential and mixed flotation and combined with the ore characteristics. This plant obtained good beneficiation indexes: lead concentrate grade reached 66.52%; the recovery rate was 88.5%.

A copper-lead-zinc ore dressing plant in Sweden with the daily output of 1000t, copper content of 0.58%, lead content of 2.85% and zinc content 4.90%; BaoShan adopted copper-lead mixed flotation. Final copper concentrate contains copper 20.25% and lead 6.75%, and the lead concentrate contains lead 58.73% and copper 3.40%.

A copper lead zinc ore dressing plant in Inner Mongolia, the mainly components of the ore are copper, lead, zinc, and a certain amount of magnetite. According to ore properties and a series of processing tests, BaoShan finally decided copper and lead mixed flotation separation - mixed tailings zinc flotation-flotation tailings weak magnetic separation process, so the plant also get more than 65% iron concentrate in addition to the grade high of copper, lead and zinc concentrate.

13607976909
  • 在线客服
  • 在线客服